Moulin Fritte M3

Description: Ancienne fritte

Oxide Analysis Formula Tolerance
CaO 8.84% 0.37
MgO 0.03% -
K2O 8.68% 0.21
Na2O 11.13% 0.42
Al2O3 9.00% 0.21
B2O3 13.55% 0.45
SiO2 48.76% 1.89
Oxide Weight 232.55
Formula Weight 232.55

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy