Description: Low iron high soda feldspar

Oxide Analysis Formula Tolerance
Na2O 9.11% 0.70
MgO 0.05% 0.01
CaO 2.95% 0.25
TiO2 0.01% -
Fe2O3 0.06% -
Al2O3 22.40% 1.04
K2O 0.89% 0.04
SiO2 63.90% 5.06
Oxide Weight 472.72
Formula Weight 472.72

Notes

This is a very low iron, high soda feldspar. It comes from a large scale feldspar mine that is very close to a port in Chennai, India. Thus the potential for quality, availability and low price to international markets is very good.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Materials MGK Alakali Feldspar
Media Mica and Feldspar Mine of MGK Minerals

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy