1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Mergal K10N

Notes

Mergal® K10N is a non-skin sensitizing BIT (Benzisothiazolinone) VOC-free industrial preservative used to prevent deterioration and degradation caused by bacteria and fungi In water-borne adhesives, sealants, and pigment slurries. In ceramics it is useful in bodies and glazes. It has low viscosity and is free of solvents and surfactants and is convenient to handle year-round.

Typical Dose: 0.05 wt. % – 0.4 wt. % (in-package protection)
Applicable to products with a range of pH 3 – 13
Heat stable to 100° C.
Add as early in production as possible.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Biocide
These are added to glazes and bodies to prevent the growth of micro organisms. Often targeted at bacteria, mold or fungi.
URLs https://www.troycorp.com/product_view_final_t.asp?cat=products&uID=1&pID=30
Mergal Biocide data sheet
A a non-skin sensitizing BIT (Benzisothiazolinone) formulation. The product is an industrial preservative used to prevent deterioration and degradation caused by bacteria and fungi in aqueous systems.
Materials Polyphase P20T

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy