| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 26.99% | 1.00 | |
| K2O | 0.05% | - | |
| Na2O | 0.03% | - | |
| B2O3 | 50.57% | 1.51 | |
| Al2O3 | 4.97% | 0.10 | |
| SiO2 | 17.40% | 0.60 | |
| Oxide Weight | 207.44 | ||
| Formula Weight | 207.44 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Calcium Borate
|
| Materials |
PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron). |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk