Lead Oxide, Boric Oxide and Silica Eutectic

Oxide Analysis Formula Tolerance
PbO 77.80% 1.00
B2O3 5.80% 0.24
SiO2 16.40% 0.78
Oxide Weight 286.89
Formula Weight 286.89

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 485C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy