Lead Fluoride

Formula: PbF2

Oxide Analysis Formula Tolerance
PbF2 100.00% 1.00
Oxide Weight 245.20
Formula Weight 245.20

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

Data

Frit Softening Point 855C