Description: Leadless High Calcia Boron Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 15.51% | 0.68 | |
| Na2O | 8.07% | 0.32 | |
| B2O3 | 31.13% | 1.10 | |
| Al2O3 | 13.27% | 0.32 | |
| SiO2 | 32.02% | 1.31 | |
| Oxide Weight | 245.92 | ||
| Formula Weight | 245.92 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |