| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.39% | 0.01 | |
| Na2O | 1.21% | 0.05 | |
| CaO | 10.55% | 0.52 | |
| PbO | 32.97% | 0.41 | |
| Al2O3 | 2.35% | 0.06 | |
| B2O3 | 14.10% | 0.56 | |
| SiO2 | 38.42% | 1.78 | |
| Oxide Weight | 278.19 | ||
| Formula Weight | 278.19 | ||
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.4 x 10-6 (50-450C) |
|---|---|
| Frit Softening Point | 1525F |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk