Godfrey Feldspar

Description: Soda feldspar

Oxide Analysis Formula Tolerance
CaO 2.86% 0.36
Na2O 5.54% 0.64
Al2O3 17.07% 1.19
SiO2 74.31% 8.81
LOI 1.50%n/a
Oxide Weight 711.01
Formula Weight 721.84

Notes

Another formula that we have is quite different from the one shown here. There is no way to verify where either one came from, however this one may be more correct since it has K2O, which it is difficult to imagine any feldspar lacking completely.

K2O 0.5
Na2O 0.4
CaO 0.1
Al2O3 1.45
SiO2 6.45

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy