Description: Potash/sodium/calcium Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.80% | 0.08 | |
| MgO | 0.05% | 0.01 | |
| K2O | 10.40% | 0.63 | |
| Na2O | 3.00% | 0.28 | |
| Al2O3 | 18.00% | 1.01 | |
| SiO2 | 67.56% | 6.45 | |
| Fe2O3 | 0.08% | - | |
| LOI | 0.16% | n/a | |
| Oxide Weight | 573.12 | ||
| Formula Weight | 574.04 | ||
G-40 is a potassium / sodium / calcium aluminum silicate used as a source of alumina and potash in specialized glass batch formulations requiring higher potassium levels. Carefully beneficiated using the froth flotation process, G-40 Feldspar offers low iron oxide and high alkali oxide content per unit of alumina.
| URLs |
http://www.zemex.com/feldspar/g40spar.html
G40 Data Sheet |
| Materials |
G-20 Feldspar
|
| Materials |
Potash Feldspar
A feldspar having a KNaO content that predominates in potassium. |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Bulk Density lbs/cu. ft. (Packed) | 90 |
|---|---|
| Sieve Analysis Dry | +30 mesh: tr +40 mesh: 0.3 +200 mesh: 94.8 |