| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 6.00% | 0.13 | |
| Na2O | 27.00% | 0.87 | |
| Al2O3 | 6.00% | 0.12 | |
| B2O3 | 12.00% | 0.35 | |
| SiO2 | 49.00% | 1.63 | |
| Oxide Weight | 200.33 | ||
| Formula Weight | 200.33 | ||
Chemistry is approximate.
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |