Fusion Frit F-280

Alternate Names: Fusion Frit F280 Fusion

Description: All fritted cone 06 glazes

Oxide Analysis Formula Tolerance
CaO 14.20% 0.68
K2O 0.60% 0.02
Na2O 7.00% 0.30
Al2O3 8.50% 0.22
B2O3 15.00% 0.58
SiO2 54.80% 2.45
Oxide Weight 268.80
Formula Weight 268.80

Notes

A popular frit used in by glaze manufacturers for the hobby ceramics market.

Related Information

Links

Materials Ferro Frit CC-250
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.9 x 10-6
Frit Softening Point 1550F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy