| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 0.45% | 0.18 | |
| CaO | 0.45% | 0.72 | |
| K2O | 0.10% | 0.10 | |
| B2O3 | 0.45% | 0.58 | |
| SiO2 | 1.50% | 2.25 | |
| Oxide Weight | 265.79 | ||
| Formula Weight | 265.79 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Softening Point | 855C |
|---|