Description: Reimbold & Strick fast firing Zn,Ca matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 13.00% | 0.22 | |
| Na2O | 6.00% | 0.16 | |
| SiO2 | 47.00% | 1.32 | |
| CaO | 14.00% | 0.42 | |
| ZnO | 20.00% | 0.42 | |
| Oxide Weight | 168.91 | ||
| Formula Weight | 168.91 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 73 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | >800C |