Frit NR 2

Alternate Names: Fritte NR 2, Frit NR2

Oxide Analysis Formula Tolerance
K2O 5.40% 0.21
CaO 11.90% 0.79
B2O3 17.60% 0.94
Al2O3 11.80% 0.43
SiO2 53.20% 3.29
Oxide Weight 370.76
Formula Weight 370.76

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 665 C