| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 25.23% | 1.07 | |
| Al2O3 | 6.06% | 0.18 | |
| Na2O | 17.16% | 0.82 | |
| K2O | 4.04% | 0.13 | |
| CaO | 1.00% | 0.05 | |
| SiO2 | 46.50% | 2.29 | |
| Oxide Weight | 296.28 | ||
| Formula Weight | 296.28 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |