Frit A 4018

Description: Reimbold & Strick fast fire high barium matte frit

Oxide Analysis Formula Tolerance
Al2O3 5.00% 0.09
K2O 3.00% 0.06
SiO2 34.00% 1.07
ZnO 21.00% 0.49
BaO 37.00% 0.45
Oxide Weight 188.26
Formula Weight 188.26

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 105 x 10-7 (20-400C)
Frit Softening Point >800C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy