1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit A 3383

Description: Reimbold & Strick high melting low exp matte frit

Oxide Analysis Formula Tolerance
ZnO 3.60% 0.20
Al2O3 22.50% 1.00
Li2O 2.60% 0.40
CaO 5.00% 0.40
SiO2 66.30% 5.00
Oxide Weight 453.31
Formula Weight 453.31

Notes

Until June 2021 the analysis shown here was approximate, this one is now more accurate.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 18 x 10-7 (20-400C)
Frit Softening Point >800C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy