Description: Reimbold & Strick copper frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 15.00% | 1.30 | |
| CaO | 2.00% | 0.22 | |
| Na2O | 4.00% | 0.39 | |
| BaO | 10.00% | 0.39 | |
| SiO2 | 49.00% | 4.93 | |
| Al2O3 | 4.00% | 0.24 | |
| Oxide Weight | 507.86 | ||
| Formula Weight | 507.86 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 53 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 640C |
| Glass Transition Temperature | 600C |