Description: Reimbold & Strick barium stoneware frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 5.00% | 0.28 | |
| Li2O | 1.00% | 0.12 | |
| CaO | 7.00% | 0.44 | |
| SiO2 | 58.00% | 3.39 | |
| B2O3 | 15.00% | 0.76 | |
| BaO | 7.00% | 0.16 | |
| Al2O3 | 7.00% | 0.24 | |
| Oxide Weight | 351.32 | ||
| Formula Weight | 351.32 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 60 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 650C |
| Glass Transition Temperature | 590C |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk