Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
Description: Reimbold & Strick lead monosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 21.20% | 1.00 | |
| PbO | 78.80% | 1.00 | |
| Oxide Weight | 283.25 | ||
| Formula Weight | 283.25 | ||
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Ferro Frit 3377
|
| Materials |
Lead Monosilicate Frit
A standard frit of 1 molar part of PbO and 1 of SiO2. It melts lower than a lead bisilicate. |
| URLs |
http://www.reimbold-und-strick.de/en/index-eng/
Reimbold & Strick website |
| Co-efficient of Linear Expansion | 90 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 470C |
| Glass Transition Temperature | 440C |