Fly Ash Type F

Notes

Flyash is what is left after the burning of coal in power generating plants. It is a fine powder.

Related Information

Brick made from Fly Ash


This picture has its own page with more detail, click here to see it.

Mix is 90% fly ash with ball clay and bentonite to make it plastic enough to form.

Oxide Analysis Formula Tolerance