Alternate Names: Frit 21 C004
Description: Alkaline Borate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 4.38% | 0.15 | |
| Na2O | 13.64% | 0.73 | |
| CaO | 1.58% | 0.09 | |
| MgO | 0.22% | 0.02 | |
| Al2O3 | 10.68% | 0.35 | |
| B2O3 | 17.06% | 0.82 | |
| SiO2 | 52.14% | 2.89 | |
| ZrO2 | 0.30% | 0.01 | |
| Oxide Weight | 333.20 | ||
| Formula Weight | 333.20 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Melting Range (C) | 900-1100C |
|---|