Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
Alternate Names: Frit 21 C001
Description: Fritte Boracique
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 17.68% | 0.61 | |
| Al2O3 | 4.78% | 0.10 | |
| B2O3 | 50.45% | 1.50 | |
| CaO | 27.09% | 1.00 | |
| Oxide Weight | 207.09 | ||
| Formula Weight | 207.09 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.1 x 10-8 C |
|---|---|
| Frit Melting Range (C) | 1050-1160C |