Description: Lead calcium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 12.30% | 0.52 | |
| K2O | 1.80% | 0.05 | |
| Na2O | 1.10% | 0.04 | |
| PbO | 37.60% | 0.40 | |
| B2O3 | 13.00% | 0.44 | |
| Al2O3 | 2.60% | 0.06 | |
| SiO2 | 31.60% | 1.24 | |
| Oxide Weight | 235.54 | ||
| Formula Weight | 235.54 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 166
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.6 |
|---|---|
| Frit Melting Range (C) | 1400F |