Description: Low Lead Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.40% | 0.58 | |
| K2O | 2.71% | 0.09 | |
| Na2O | 1.78% | 0.09 | |
| PbO | 17.12% | 0.24 | |
| B2O3 | 8.01% | 0.36 | |
| Al2O3 | 6.19% | 0.19 | |
| SiO2 | 53.78% | 2.80 | |
| Oxide Weight | 312.87 | ||
| Formula Weight | 312.87 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Pemco Frit Pb-2G30
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk