Description: High lead borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 63.30% | 1.00 | |
| B2O3 | 19.80% | 1.00 | |
| SiO2 | 16.90% | 0.99 | |
| Oxide Weight | 352.61 | ||
| Formula Weight | 352.61 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 4GF63D
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.0 |
|---|---|
| Frit Melting Range (C) | 1050F |