Description: Leadless calcium potassium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.20% | 0.38 | |
| K2O | 7.00% | 0.31 | |
| MgO | 1.99% | 0.20 | |
| Na2O | 1.63% | 0.11 | |
| B2O3 | 4.70% | 0.28 | |
| Al2O3 | 15.10% | 0.61 | |
| SiO2 | 64.39% | 4.41 | |
| Oxide Weight | 412.12 | ||
| Formula Weight | 412.12 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.60 |
|---|---|
| Frit Melting Range (C) | 1900F |