Description: Netherland, Flanders area (Ferro?)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.18% | 0.43 | |
| B2O3 | 6.42% | 0.31 | |
| SiO2 | 54.20% | 3.03 | |
| Al2O3 | 6.07% | 0.20 | |
| Na2O | 2.03% | 0.11 | |
| K2O | 3.93% | 0.14 | |
| MgO | 0.24% | 0.02 | |
| PbO | 19.93% | 0.30 | |
| Oxide Weight | 335.91 | ||
| Formula Weight | 335.91 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |