Description: Alkali borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 15.60% | 1.00 | |
| Al2O3 | 5.10% | 0.20 | |
| B2O3 | 26.30% | 1.50 | |
| SiO2 | 52.90% | 3.50 | |
| Oxide Weight | 397.04 | ||
| Formula Weight | 397.04 | ||
This is not a replacement for Colemanite as claimed by some.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |