Description: DK-2, DK-3, RC100
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 0.03% | 1.00 | |
| Fe2O3 | 0.04% | 0.85 | |
| SiO2 | 0.04% | 2.26 | |
| ZrO2 | 99.50% | ||
| TiO2 | 0.10% | 4.26 | |
| Oxide Weight | 339,014.00 | ||
| Formula Weight | 339,014.00 | ||
Particle size ranges from 0.90 microns to 8.0 microns, surface area from 3 to 100 grams to square meter.
Stabilized, partially stabilized and doped zirconias also available.
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |