DF Cornwall Stone

Oxide Analysis Formula Tolerance
CaO 0.20% 0.03
K2O 3.80% 0.38
Na2O 3.90% 0.59
Al2O3 12.01% 1.10
SiO2 79.57% 12.40
Fe2O3 0.06% -
LOI 0.45%n/a
Oxide Weight 931.95
Formula Weight 936.17

Notes

Defluorinated or DF Cornwall Stone is a processed material, micaceous iron and fluorine are removed by a flotation process.

Related Information

Links

Materials Cornwall Stone
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy