Degussa Frit 90208M

Oxide Analysis Formula Tolerance
Na2O 25.10% 0.90
K2O 4.00% 0.09
CaO 0.10% -
Al2O3 11.80% 0.26
SiO2 58.80% 2.18
Oxide Weight 222.23
Formula Weight 222.23

Notes

This frit is referenced in the book "Macro-Crystalline Glazes" by Peter Ilsley.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.