Description: High boron sodium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 65.45% | 6.37 | |
| Na2O | 10.60% | 1.00 | |
| B2O3 | 23.95% | 2.01 | |
| Oxide Weight | 584.91 | ||
| Formula Weight | 584.91 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Melting Range (C) | 980-1080C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk