| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.32% | 0.02 | |
| K2O | 1.45% | 0.04 | |
| MgO | 0.71% | 0.05 | |
| Na2O | 0.16% | 0.01 | |
| TiO2 | 2.06% | 0.07 | |
| Al2O3 | 38.22% | 1.00 | |
| P2O5 | 0.08% | - | |
| SiO2 | 55.40% | 2.46 | |
| Fe2O3 | 1.56% | 0.03 | |
| SO3 | 0.03% | n/a | |
| Oxide Weight | 266.77 | ||
| Formula Weight | 266.85 | ||
| Materials |
Fireclay
|
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |
| Typecodes |
Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more. |