Description: Potash Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.03 | |
| K2O | 8.50% | 0.58 | |
| Na2O | 3.75% | 0.39 | |
| Al2O3 | 16.34% | 1.03 | |
| SiO2 | 70.75% | 7.54 | |
| Fe2O3 | 0.07% | - | |
| LOI | 0.29% | n/a | |
| Oxide Weight | 638.90 | ||
| Formula Weight | 640.76 | ||
Mined in Chesterfield County, Virginia.
| Materials |
Custer Feldspar (pre-2000)
The most common potash feldspar used in ceramics in North America, a standard for many decades, but no longer available. Its chemistry shifted around 2000. |
| Materials |
G-200 Feldspar
|
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |