Ceradel Frit C 1255

Alternate Names: Fritte C1255, Fritte C 1255, Ceradel Frit 1255

Description: Fritte zirconifere sans plomb, low expansion ziron frit

Oxide Analysis Formula Tolerance
Al2O3 5.62% 0.20 3
Na2O 2.70% 0.16 2
K2O 4.10% 0.16 2
B2O3 12.11% 0.63 2.5
SiO2 55.75% 3.33 15
ZnO 7.08% 0.31 2.5
ZrO2 6.79% 0.20 2.5
CaO 5.85% 0.37 2
Oxide Weight 359.29
Formula Weight 359.29

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 58x10-7 (20/300C)
Frit Softening Point 920-1020C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy