Ca Biborate and Ca Metaborate Eutectic

Oxide Analysis Formula Tolerance
CaO 34.80% 1.00
B2O3 65.20% 1.51
Oxide Weight 161.21
Formula Weight 161.21

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 990C