Description: SODA FELDSPAR
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.70% | 0.07 | |
| K2O | 5.19% | 0.31 | |
| MgO | 0.06% | 0.01 | |
| Na2O | 6.89% | 0.62 | |
| Al2O3 | 18.48% | 1.01 | |
| SiO2 | 68.43% | 6.32 | |
| Fe2O3 | 0.06% | - | |
| LOI | 0.24% | n/a | |
| Oxide Weight | 553.91 | ||
| Formula Weight | 555.24 | ||
| Materials |
F-4 Feldspar
|
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |