1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Bangalore Quartz

Description: Quartz, Flint, Silica

Oxide Analysis Formula Tolerance
Al2O3 0.04% 1.00
SiO2 99.82%
Fe2O3 0.04% 0.64
LOI 0.10%n/a
Oxide Weight 254,745.00
Formula Weight 255,000.00

Notes

A raw material mined in India.

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.