Ba Metaborate and Ba Pyroborate Eutectic

Oxide Analysis Formula Tolerance
BaO 77.40% 1.00
B2O3 22.60% 0.64
Oxide Weight 198.06
Formula Weight 198.06

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 750C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy