| Monthly Tech-Tip | No tracking! No ads! | |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.22% | 0.01 | |
| MgO | 0.05% | - | |
| Na2O | 0.01% | - | |
| TiO2 | 1.76% | 0.06 | |
| Al2O3 | 39.21% | 1.00 | |
| P2O5 | 0.10% | - | |
| SiO2 | 44.73% | 1.94 | |
| Fe2O3 | 0.37% | 0.01 | |
| LOI | 13.55% | n/a | |
| Oxide Weight | 224.89 | ||
| Formula Weight | 260.14 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk