Lead Chromate

Alternate Names: Lead(II) Chromate

Oxide Analysis Formula Tolerance
PbO 67.45% 1.00
CrO3 32.55% 1.08
Oxide Weight 330.91
Formula Weight 330.91

Notes

In nature lead chromate exists as the mineral crocoite. It has monoclinic brilliant-red to orange prismatic crystals. Crocoite decomposes below 1000 degrees to lead oxide and green chromic oxide.

The brilliant reds, oranges, vermillion, and yellow colours achieved in lead-chromium glazes are due to precipitation of crocoite crystals. However lead chromate material is very toxic.

Related Information

Links

Hazards Lead Chromate
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy