Basalt

Oxide Analysis Formula Tolerance
CaO 7.90% 0.32
K2O 0.60% 0.01
MgO 10.30% 0.58
Na2O 2.40% 0.09
TiO2 1.60% 0.05
Al2O3 14.10% 0.31
P2O5 0.30% -
SiO2 48.60% 1.82
Fe2O3 11.20% 0.16
MnO 0.10% -
LOI 3.80%n/a
Oxide Weight 218.89
Formula Weight 227.54

Notes

Volcanic rock essentially of plagioclase, labradorite, magnetite, and pyroxene, with olivine, biotite, and hornblende. Formed by magma emission. There are two distinct basalts: feldspathic and alkaline, both plagioclase feldspathics but the latter containing significantly more sodium and potassium.

Related Information


This picture has its own page with more detail, click here to see it.

Basalt


This picture has its own page with more detail, click here to see it.

Peridot In Basalt


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy