Description: KAOLINIZED SAND
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.22% | 0.03 | |
| K2O | 2.93% | 0.25 | |
| MgO | 0.36% | 0.07 | |
| Na2O | 0.36% | 0.05 | |
| TiO2 | 0.49% | 0.05 | |
| Al2O3 | 12.46% | 1.00 | |
| P2O5 | 0.05% | - | |
| SiO2 | 79.44% | 10.82 | |
| Fe2O3 | 0.73% | 0.04 | |
| MnO | 0.02% | - | |
| LOI | 3.71% | n/a | |
| Oxide Weight | 794.55 | ||
| Formula Weight | 825.17 | ||
Pre-96 Analysis.
CaO... 0.22
K2O... 2.93
MgO... 0.36
Na2O.. 0.36
TiO2.. 0.49
Al2O3. 12.46
SiO2.. 79.44
Fe2O3. 0.73
LOI... 3.71
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |