Description: Soda feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 2.86% | 0.36 | |
| Na2O | 5.54% | 0.64 | |
| Al2O3 | 17.07% | 1.19 | |
| SiO2 | 74.31% | 8.81 | |
| LOI | 1.50% | n/a | |
| Oxide Weight | 711.01 | ||
| Formula Weight | 721.84 | ||
Another formula that we have is quite different from the one shown here. There is no way to verify where either one came from, however this one may be more correct since it has K2O, which it is difficult to imagine any feldspar lacking completely.
K2O 0.5
Na2O 0.4
CaO 0.1
Al2O3 1.45
SiO2 6.45
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |