| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.11% | 0.01 | |
| MgO | 0.06% | 0.01 | |
| Al2O3 | 18.69% | 1.00 | |
| SiO2 | 74.76% | 6.79 | |
| Fe2O3 | 0.22% | 0.01 | |
| LOI | 6.16% | n/a | |
| Oxide Weight | 512.13 | ||
| Formula Weight | 545.75 | ||
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |