Alternate Names: Frit Pb2V93
Description: Boron-free, zinc bearing leaded dinnerware glaze cone 4
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.20% | 0.30 | |
| K2O | 2.60% | 0.07 | |
| Na2O | 1.00% | 0.04 | |
| PbO | 26.50% | 0.32 | |
| ZnO | 7.90% | 0.26 | |
| Al2O3 | 5.40% | 0.14 | |
| SiO2 | 50.30% | 2.26 | |
| Oxide Weight | 269.98 | ||
| Formula Weight | 269.98 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.60 |
|---|---|
| Co-efficient of Linear Expansion | 6.6 x 10-6 (50-450C) |
| Frit Softening Point | 1560F |
| Frit Melting Range (C) | 1530-1650F |
| I.F.P. (celsius) | 598C |