Pemco Frit Pb-1N86

Alternate Names: Frit Pb1N86

Description: Cone 1 glaze with 50% clay addition

Oxide Analysis Formula Tolerance
CaO 3.90% 0.23
Na2O 12.60% 0.68
PbO 5.80% 0.09
B2O3 28.20% 1.36
SiO2 49.50% 2.76
Oxide Weight 334.75
Formula Weight 334.75

Notes

Developed for sewer pipe

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.10
Co-efficient of Linear Expansion 8.1 x 10-6 (50-450C)
Frit Softening Point 1300F
Frit Melting Range (C) 1280-1380F
I.F.P. (celsius) 595C
By Tony Hansen