Alternate Names: PotteryCrafts Frit 2962
Description: High alkaline very high expansion frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 6.90% | 0.09 | |
| CaO | 2.90% | 0.10 | |
| K2O | 10.30% | 0.22 | |
| Na2O | 18.60% | 0.59 | |
| Al2O3 | 5.30% | 0.10 | |
| B2O3 | 3.40% | 0.10 | |
| SiO2 | 52.50% | 1.73 | |
| Oxide Weight | 197.41 | ||
| Formula Weight | 197.41 | ||
We have found other chemistries but this is from the PotteryCrafts website.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information |
| Co-efficient of Linear Expansion | 13.4 |
|---|---|
| Frit Melting Range (C) | 880-1060C |
| By Tony Hansen Follow me on ![]() | ![]() |